The Hotline Public Forum for Anodizing
Nut with black zinc coating fails 96 hour salt spray test January 18 40095. White layer forms during acid zinc plating but not on Hull Cell panels open Q. January 18 35543. Porosity problems in hard chrome plating open Q. January 18 02412. Electrolytic gold plating is immersion depositing on non electrified housing January 17 53207.