The Study of Copper Anodes in Acid and Cyanide Plating
16/09/2015· A high efficiency potassium cyanide solution with a wetting agent was used in 15 gallon pilot plant tanks, arranged in electrical series for evaluating the different anodes simultaneously. The formulation and conditions for this solution are summarized in Tables 3 and 4. The tanks were operated for 20 days 3600 A hr with direct current and for another 20 days 4120 A hr with the current